  • Ertacetal® C

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 165  °C
    thermal conductivity 0.31  W/(K*m)
  • Ertalon® 6 SA

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 220  °C
    thermal conductivity 0.28  W/(K*m)
  • Ertalyte®

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 245  °C
    thermal conductivity 0.29  W/(K*m)
  • Ertalyte® TX

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 245  °C
    thermal conductivity 0.29  W/(K*m)
  • Ketron® TX PEEK

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 340  °C
    thermal conductivity 0.25  W/(K*m)
  • Ketron® 1000 PEEK

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 340  °C
    thermal conductivity 0.25  W/(K*m)
  • Techtron® HPV PPS

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 280  °C
    thermal conductivity 0.3  W/(K*m)
  • TIVAR® 1000

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • TIVAR® 1000 antistatic

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • TIVAR® 1000 ASTL

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • TIVAR® 1000 EC

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • TIVAR® Cleanstat

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • TIVAR® DS

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • TIVAR® H.O.T.

    Mitsubishi Chemical Advanced Materials

    category plastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(K*m)
  • APSOplast® PE-UHMW blau (Polyethylen ultra high molecular weight)

    Angst+Pfister GmbH

    category thermoplastics
    melting temperature 135  °C
    thermal conductivity 0.4  W/(m*K)
  • APSOplast® PEEK natur (braun-grau) (Polyetheretherketon)

    Angst+Pfister GmbH

    category thermoplastics
    melting temperature 343  °C
    thermal conductivity 0.25  W/(m*K)
  • APSOplast® PEEK natur (braun-grau) (Polyetheretherketon)

    Angst+Pfister GmbH

    category thermoplastics
    melting temperature 341  °C
    thermal conductivity 0.27  W/(m*K)

Application areas

  1. bearings
  2. spaceflight
  3. glazing
  4. food contact 32
  5. construction 17
  6. seals 17
  7. electronics 13
  8. beverage industry 11

certificate

  1. Verordnung (EG) 1935/2004
  2. FDA (CFR Title 21) 14
  3. 3-A Sanitary 6
  4. REACH (Verordnung (EG) 1907/2006) 3
  5. RoHS (Richtlinie 2011/65/EU) 3
  6. Verordnung (EG) 2023/2006 3
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code