  • Acetron® MD

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 155  MPa
    application temperature < 90  °C
  • Ertacetal® C

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 140  MPa
    application temperature < 100  °C
  • Ertalon® 6 SA

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 150  MPa
    application temperature < 70  °C
  • Ertalyte®

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 170  MPa
    application temperature < 100  °C
  • Ertalyte® TX

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 160  MPa
    application temperature < 100  °C
  • Ketron® TX PEEK

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 195  MPa
    application temperature < 250  °C
  • Ketron® 1000 PEEK

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 210  MPa
    application temperature < 250  °C
  • Nylatron® MD

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 170  MPa
    application temperature < 70  °C
  • Techtron® HPV PPS

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 160  MPa
    application temperature < 220  °C
  • TIVAR® 1000

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 33  MPa
    application temperature < 80  °C
  • TIVAR® 1000 antistatic

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 34  MPa
    application temperature < 80  °C
  • TIVAR® 1000 ASTL

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 34  MPa
    application temperature < 80  °C
  • TIVAR® 1000 EC

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 35  MPa
    application temperature < 80  °C
  • TIVAR® Cleanstat

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 33  MPa
    application temperature < 80  °C
  • TIVAR® DS

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 31  MPa
    application temperature < 80  °C
  • TIVAR® H.O.T.

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 31  MPa
    application temperature < 110  °C
  • TIVAR® MD

    Mitsubishi Chemical Advanced Materials

    category plastics
    ball indentation hardness 30  MPa
    application temperature < 80  °C
  • APSOplast® PEEK natur (braun-grau) (Polyetheretherketon)

    Angst+Pfister GmbH

    category thermoplastics
    ball indentation hardness 230  MPa
    application temperature -60 – 250  °C
  • APSOplast® PEEK natur (braun-grau) (Polyetheretherketon)

    Angst+Pfister GmbH

    category thermoplastics
    ball indentation hardness 253  MPa
    application temperature < 260  °C

Application areas

  1. construction
  2. functional models
  3. interior finishing
  4. textile industry
  5. food contact 32
  6. seals 17
  7. bearings 15
  8. electronics 13
  9. beverage industry 11

certificate

  1. Verordnung (EG) 1935/2004
  2. FDA (CFR Title 21) 16
  3. 3-A Sanitary 6
  4. REACH (Verordnung (EG) 1907/2006) 2
  5. RoHS (Richtlinie 2011/65/EU) 2
  6. Verordnung (EG) 2023/2006 2
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code