Material Hub > Materials

Materials

  • SUSTAKON®

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 70  MPa
    melting temperature 225  °C
  • SUSTAMID® 6 ESD 60

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 72  MPa
    melting temperature 222  °C
  • SUSTAMID® 6 GC

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 80  MPa
    melting temperature 220  °C
  • SUSTAMID® 6 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 80  MPa
    melting temperature 220  °C
  • SUSTAMID® 6

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 80  MPa
    melting temperature 220  °C
  • SUSTAMID® 12

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 50  MPa
    melting temperature 178  °C
  • SUSTAMID® 46

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 95  MPa
    melting temperature 295  °C
  • SUSTAMID® 66

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 85  MPa
    melting temperature 260  °C
  • SUSTAMID® 12 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 60  MPa
    melting temperature 178  °C
  • SUSTAMID® 12 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 50  MPa
    melting temperature 178  °C
  • SUSTAMID® 6 GC MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 80  MPa
    melting temperature 220  °C
  • SUSTAMID® 6 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 100  MPa
    melting temperature 220  °C
  • SUSTAMID® 66 FG

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 85  MPa
    melting temperature 260  °C
  • SUSTAMID® 66 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 100  MPa
    melting temperature 260  °C
  • SUSTAMID® 66 GLD 240

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 65  MPa
    melting temperature 260  °C
  • SUSTAMID® 66 HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 85  MPa
    melting temperature 260  °C
  • SUSTAMID® 66 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 90  MPa
    melting temperature 260  °C
  • SUSTAMID® 6G GK

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 70  MPa
    melting temperature 218  °C
  • SUSTAMID® 6G HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 75  MPa
    melting temperature 216  °C
  • SUSTAMID® 6G LU

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile stress at yield 70  MPa
    melting temperature 214  °C

Application areas

  1. mechanical engineering
  2. transportation
  3. mechanics 57
  4. electrics 36
  5. conveyor technology 26
  6. food contact 23
  7. aviation 22

producer

  1. Röchling Sustaplast SE & Co. KG
  2. Mittelrheinische Metallgießerei H. Beyer GmbH & Co. KG 34
  3. Röchling Engineering Plastics SE & Co. KG 30
  4. Röchling Engineering Plastics 20
  5. Röchling Maywo GmbH 8
  6. Angst+Pfister GmbH 6
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code