Material Hub > Materials
Materials
-
category cast steeltensile strain at break > 35 %tensile strength > 485 MPa
-
category cast steeltensile strain at break > 30 %tensile strength > 485 MPa
-
category steelstensile strain at break > 4 %tensile strength > 320.3 MPa
-
category Aluminiumtensile strain at break > 3 %tensile strength 235 – 373 MPa
-
category Kupfertensile strain at break 12 – 17 %tensile strength 620 – 725 MPa
-
category Nickeltensile strain at break > 15 %tensile strength > 1000 MPa
-
category structural steelstensile strain at break > 22 %tensile strength 430 – 630 MPa
-
category structural steelstensile strain at break > 22 %tensile strength 430 – 630 MPa
-
category structural steelstensile strain at break > 16 %tensile strength 510 – 720 MPa
-
category structural steelstensile strain at break > 21 %tensile strength 450 – 630 MPa
-
category structural steelstensile strain at break > 18 %tensile strength 500 – 680 MPa
-
category structural steelstensile strain at break > 18 %tensile strength 500 – 680 MPa
-
category structural steelstensile strain at break > 16 %tensile strength 510 – 720 MPa
-
category structural steelstensile strain at break > 17 %tensile strength 490 – 610 MPa
-
category steelstensile strain at break > 9 %tensile strength 450 – 2100 MPa
-
category steelstensile strain at break > 12 %tensile strength 450 – 2100 MPa
-
category steelstensile strain at break > 12 %tensile strength 490 – 2100 MPa
-
category steelstensile strain at break > 30 %tensile strength 580 – 800 MPa
-
category steelstensile strain at break > 30 %tensile strength 550 – 790 MPa
-
category steelstensile strain at break > 20 %tensile strength 380 – 560 MPa