Material Hub > Materials
Materials
-
category cast steeltensile strain at break > 35 %tensile strength > 485 MPa
-
category cast steeltensile strain at break > 30 %tensile strength > 485 MPa
-
category Kupfertensile strain at break 3 – 66 %tensile strength 305 – 695 MPa
-
category Kupfertensile strain at break > 12 %tensile strength > 205 MPa
-
category Kupfertensile strain at break > 12 %tensile strength > 760 MPa
-
category Kupfertensile strain at break > 10 %tensile strength > 205 MPa
-
category Kupfertensile strain at break > 6 %tensile strength > 515 MPa
-
category Kupfertensile strain at break > 5 %tensile strength > 620 MPa
-
category Kupfertensile strain at break > 15 %tensile strength > 585 MPa
-
category Kupfertensile strain at break > 2 %tensile strength 280 – 1200 MPa
-
category Kupfertensile strain at break > 2 %tensile strength 275 – 1200 MPa
-
category Kupfertensile strain at break > 2 %tensile strength 245 – 1200 MPa
-
category Kupfertensile strain at break > 2 %tensile strength 140 – 420 MPa
-
category Kupfertensile strain at break > 2 %tensile strength 140 – 698.2 MPa
-
category cast steeltensile strain at break > 20 %tensile strength 490 – 690 MPa
-
category cast steeltensile strain at break > 20 %tensile strength 480 – 650 MPa
-
category cast steeltensile strain at break > 12 %tensile strength 600 – 800 MPa
-
category cast steeltensile strain at break > 12 %tensile strength 650 – 1100 MPa
-
category cast steeltensile strain at break > 10 %tensile strength 820 – 1200 MPa
-
category cast steeltensile strain at break > 10 %tensile strength 650 – 1000 MPa