Rhenolub® MK I (GR) (einem organischen Bindeharz mit Molybdändisulfid und Graphit)
Rhenotherm Kunststoffbeschichtungs GmbH
category Kunststoffbeschichtungtensile strain at break –tensile modulus of elasticity – -
category plasticstensile strain at break 40 %tensile modulus of elasticity –
-
category plasticstensile strain at break > 50 %tensile modulus of elasticity 200 MPa
-
category plasticstensile strain at break > 50 %tensile modulus of elasticity 250 MPa
-
category plasticstensile strain at break > 50 %tensile modulus of elasticity 1300 MPa
-
category plasticstensile strain at break > 50 %tensile modulus of elasticity 1100 MPa
-
category plasticstensile strain at break > 50 %tensile modulus of elasticity 1300 MPa
-
category steelstensile strain at break > 6 %tensile modulus of elasticity 193 – 199 GPa
-
category steelstensile strain at break > 7 %tensile modulus of elasticity 184 GPa
-
category Kupfertensile strain at break –tensile modulus of elasticity 114.3 – 130.1 GPa
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity 117.2 GPa
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity 103 GPa
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity –
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity –
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity 107.9 GPa
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity 107.9 – 130.1 GPa
-
category Kupfertensile strain at break > 2 %tensile modulus of elasticity 117.2 GPa
-
category cast steeltensile strain at break > 10 %tensile modulus of elasticity 216 GPa
-
category cast irontensile strain at break –tensile modulus of elasticity –
-
category Nickeltensile strain at break > 15 %tensile modulus of elasticity 199.95 – 211 GPa