category thermoplasticsdensity 1.49 g/cm³coefficient of linear thermal expansion 0.0001 1/K
-
category thermoplasticsdensity 1.44 g/cm³coefficient of linear thermal expansion 5.0E-5 1/K
-
Geschlossenzelliger Aluminiumschaum (pulvermetallurgisches Verfahren)
Fraunhofer IWU, Abteilung Leichtbau, Textiltechnologien und Circular Economy
category zellularer Werkstoffdensity 0.7 g/cm³coefficient of linear thermal expansion 23.9 (10⁻⁶/K) -
Geschlossenzelliger Aluminiumschaum (schmelzmetallurgisches Verfahren)
Fraunhofer IWU, Abteilung Leichtbau, Textiltechnologien und Circular Economy
category zellularer Werkstoffdensity 0.25 g/cm³coefficient of linear thermal expansion 21 – 23 (10⁻⁶/K) -
Offenzelliger Aluminiumschaum (schmelzmetallurgisches Verfahren)
Fraunhofer IWU, Abteilung Leichtbau, Textiltechnologien und Circular Economy
category zellularer Werkstoffdensity 0.16 g/cm³coefficient of linear thermal expansion 22 – 24 (10⁻⁶/K) -
category plasticsdensity 1.32 g/cm³coefficient of linear thermal expansion 40 10⁻⁶/K
-
category plasticsdensity 1.79 g/cm³coefficient of linear thermal expansion 140 10⁻⁶/K
-
category plasticsdensity 1.78 g/cm³coefficient of linear thermal expansion 140 10⁻⁶/K
-
category plasticsdensity 1.4 g/cm³coefficient of linear thermal expansion 130 10⁻⁶/K
-
category plasticsdensity 1.34 g/cm³coefficient of linear thermal expansion 170 10⁻⁶/K
-
category plasticsdensity 1.64 g/cm³coefficient of linear thermal expansion 60 – 80 10⁻⁶/K
-
category plasticsdensity 1.4 g/cm³coefficient of linear thermal expansion 60 – 80 10⁻⁶/K
-
category plasticsdensity 1.78 g/cm³coefficient of linear thermal expansion –
-
category plasticsdensity 1.33 g/cm³coefficient of linear thermal expansion –
-
category plasticsdensity 0.95 g/cm³coefficient of linear thermal expansion 150 – 230 10⁻⁶/K
-
category plasticsdensity 0.92 g/cm³coefficient of linear thermal expansion 120 – 190 10⁻⁶/K
-
category plasticsdensity 0.92 g/cm³coefficient of linear thermal expansion 120 – 190 10⁻⁶/K
-
category plasticsdensity 1.78 g/cm³coefficient of linear thermal expansion 100 – 140 10⁻⁶/K
-
category plasticsdensity 1.78 g/cm³coefficient of linear thermal expansion 100 – 140 10⁻⁶/K
-
category plasticsdensity 1.71 g/cm³coefficient of linear thermal expansion 90 10⁻⁶/K